Tensile Testing
Hardness Testing
Impact Testing
Bend Testing
Fatigue Testing
 

 

 

 

Tensile Testing

The Metallurgical Engineering Services test lab offers tensile tests on all metals, polymers, composites, and fabrics.  Tensile testing is the most fundamental type of mechanical testing.  A tensile test applies a proof load to a specimen past the yield point to failure.  Tensile test results provide many mechanical properties such as Young's modulus, yield strength, tensile strength, elongation, deformation, reduction of area, and strain hardening behavior. 

Specimens may be dog bone tensile bars or a variety of other shapes.   We routinely test machined coupons, fasteners, wire, cable, tubes, pipes, plates, structural beams, or bars.  Our machine shop and qualified machinists will machine your raw materials to standard coupons if necessary.  We utilize an extensive variety of grips and fixtures to provide the tensile setup needed to complete your test. 

Specifications for tests performed may be ASTM, MIL, or other standards.  The experience of our engineers and a comprehensive quality control program ensure accurate, reproducible results.  

Temperatures for tensile tests may be reduced to -100F or elevated 1500F.

Our primary mechanical testing instrumentation includes the following:

  • Satec, Model 120HVL, 120,000lb capacity, Servo Hydraulic
  • Baldwin, Model TEG, 60,000lb capacity, Hydraulic
  • Instron, Model 1000, 1000lb capacity, Screw Driven
  • Brinell Hardness Tester, Model L
  • Rockwell Hardness Tester, Wilson Model 4DT
  • Vickers Micro Hardness Tester, Model LR, Tukon Model 300BM 
  • Knoop Micro Hardness Tester, Tukon Model 300BM
  • Durometer Hardness Tester, Types A & D, Instron Model 1600 (2)
  • Charpy Impact Tester, Model CS-137-074
  • Friction & Wear Tester, Paul N. Gardner Co. Model 80
  • Taber Abrasion Tester, Model 503-1
  • Paint Adhesion Tester
  • Digital Strain Gage data display
  • 14' Drop Impact Tower
  • Satec Model R.R. Moore Fatigue Tester

MES is capable of testing large lot sizes for manufacturing controls and we offer discounted rates for high volume testing.  

 

 

News & Highlights

48 Hour Rapid Turnaround options are available

ISO 9001:2000 Certified


 

 

 

 
 Copyright © 2006 Metallurgical Engineering Services | Home | Site Map | Request Quote | Books and Software | Top Page 1